LINER COMPARISON B
|
PetroGard
VI |
PetroGard X |
HDPE |
|
Thickness (Mils) ASTM-D-751
|
30 |
40 |
60 |
|
Puncture Resistance (Lbs.) ASTMD-751 (Ball Tip)
|
950 |
1500 |
330 |
|
Base Fabric Weight Method 5041 oz/sq. yd.
|
7.5 |
13 |
n/a |
|
Tensile at Break(Lbs.) ASTMD-638 Type IV |
485 |
1100 |
240 |
|
Tensile at Yield 1100 (Lbs.) ASTMD-638 Type IV |
485 |
1100 |
140 |
|
Rate of Thermal Expansion/Contraction
(in./100'/150ºF)
|
.78 |
78 |
17.6 |
|
Permeability JP8 (oz/ft2/24 hr.) |
.015 |
.0024 |
.05 |
|
|
|