MATERIAL SPECIFICATION


Thickness - in.
(ASTM D-751)
35 mil
Base - (Type)Nylon
Fabric - (Weight)13 oz./sq.yd.
Finished Coated Weight
(ASTM D751)
32 +/- 3 oz./sq. yd. min.
Tongue Tear
(ASTM D-751)
40/40 lbs. (min)
Strip tensile lbs.
(ASTM D-751) Cut strip method
700 lbs/600 lbs
Adhesion (
ASTM D751)
30 lbs/in.
Hydrostatic Resistance
(ASTM D751 Method A Proc. 1)
600 psi min.
Low Temperature
ASTM D-2136 1" Mandrel 4 hrs.
Pass -50E F
Puncture Resistance
ASTM D-751 (Ball tip)
1200 lbs.
Dead Load Seam Strength 2" overlap seam
Room Temperature200 lbs./in
160E F/71E C.100 lbs./in
Permeability JP-80.12 fl.oz./sq. ft./24 hr.